Cut film, not ground pigment

Glitter for injection molding starts as film, not powder. Producers metallize PET film or aluminum foil, then precision-cut it into discrete hexagonal flakes. Molding grades typically measure 100–600 μm across on carriers around 25–50 μm thick. Each flake acts as a small flat mirror, so a molded part sparkles from thousands of sharp reflection points. A dye or pigment particle can never do that. It has no facet. Silver remains the volume grade; gold, colored and holographic films widen the palette by tinting the carrier or embossing it with a diffraction pattern.

The same logic separates glitter from pearlescent pigment. Glitter is a cut specular reflector, bright and discrete. A pearlescent grade is a mica or synthetic platelet coated with titanium dioxide layers a fraction of a micrometer thick, and its color travels with viewing angle through thin-film interference. The coating side of that split is covered in our guide to pearlescent pigments in coatings; the flake side, including glitter for molding, sits in the same effect pigments catalog.

Heat resistance: match the flake to the melt

Glitter injection molding succeeds or fails on one decision, the flake carrier. Metallized PET glitter is typically rated around 160–200 °C, the region where the film softens enough to curl a flake and dull its facet. Aluminum-foil glitter is commonly quoted near 300 °C. Judge both numbers against melt temperature. Melt contact, not mold contact, is what attacks the flake.

Resin / process Typical melt or cure range Metallized PET glitter (≈160–200 °C) Aluminum glitter (≈300 °C)
LDPE 140–180 °C Comfortable Comfortable
Rigid PVC 160–190 °C Comfortable Comfortable
PP 180–220 °C Comfortable, short dwell Comfortable
PS 180–230 °C Workable Comfortable
ABS 210–250 °C Marginal, short dwell Workable
PA6 240–280 °C Not recommended Workable, short dwell
PC 280–320 °C Not recommended Marginal, large gate
Epoxy / phenolic molding 150–175 °C Comfortable Comfortable

Epoxy and phenolic compounds earn their row. Transfer and compression molding cure at roughly 150–175 °C, well inside the PET window, which is why glitter surfaces on instrument knobs, cosmetic closures and electrical accessories among the typical molding applications we supply.

How to keep facets alive in the barrel

Glitter normally enters the press in a masterbatch, let down at about 1–4%. Moderate screw speed and low back pressure preserve flatness; heavy shear folds flakes and the sparkle reads dull. Geometry matters as much as heat. A working rule is to keep flake diameter well below both the gate opening and the thinnest wall, or packing pressure will orient flakes into visible flow lines. Residence time counts as well. A melt parked in the barrel for long soaks at the top of the PET window shows edge curl even when the temperature number looked safe.

Solvent and chemical resistance

PET shrugs off water, alcohols, dilute acids and most hydrocarbon solvents, so ordinary cleaning leaves the flake untouched. The vulnerable part is the mirror. Strong alkali and some aggressive acidic cleaners etch aluminum, and the sparkle grays out over repeated exposure. Parts destined for cosmetics or household chemicals deserve a flake specified for acid and alkali resistance, a property our glitter listing carries alongside heat and solvent resistance.

Before a tool runs, run a wipe. Rub a molded plaque 20–50 times with a cloth soaked in ethanol or MEK, then inspect under magnification for flake loss, bleed or tarnish. A surface that holds up through fifty rubs without change is generally considered safe for household service. A failure points at the flake carrier or the masterbatch carrier resin, not the base polymer.

Frequently asked questions

Can PET glitter survive polycarbonate or nylon melts?
Usually not. PC runs at 280–320 °C and PA6 at 240–280 °C, past the typical 160–200 °C rating of metallized PET. For these resins the workable combination is aluminum-foil glitter near its 300 °C rating, minimal residence time and a generous gate.

What flake size suits injection molding best?
Most molders stay between 100 and 600 μm. Larger flakes sparkle harder but demand larger gates and thicker walls. Below about 100 μm the effect reads as a soft shimmer rather than glitter.

Does glitter weaken the molded part?
At a typical dose of 1–4% the effect is small, comparable to a low-level filler. Keep flakes well under wall thickness and avoid packing pressure spikes, and tensile results barely move.

About Ultra Color

Ningbo Ultra Color supplies glitter alongside solvent dyes, organic and inorganic pigments and additives for the plastic, coating and ink industries. Every lot is screened against REACH SVHC and RoHS requirements, and a retention sample from each batch is kept for 5 years. Bring the resin and melt temperature; the flake choice follows from there.

Scroll to Top