Two defense lines against sunlight

Outdoor failure of a plastic part usually starts between 290 and 400 nanometers. Photons in that band cleave polymer chains and set off radical oxidation; a season later the surface chalks, yellows and embrittles while the pigment underneath still tests fine. Formulators counter with two additive families. UV absorbers and HALS (hindered amine light stabilizers) attack the problem from opposite ends: the absorber intercepts incoming light, while the stabilizer interrupts the radical chemistry that any escaping photons trigger. The mechanisms differ, and weatherable compounds usually carry both.

How UV absorbers convert light into heat

UV absorbers rely on an intramolecular hydrogen bond that opens a ready energy pathway, with benzotriazoles and benzophenones dominating the class. The molecule takes in a UV photon, typically anywhere in the 300–380 nm range, holds the energy briefly in an excited state, then releases it to the polymer as a trace of heat. The molecule is not consumed. Protection does follow the Beer–Lambert law: it scales with concentration and with optical path, which is why thick sections benefit far more than thin films.

UV-P: the compact benzotriazole

UV-P (2-(2H-benzotriazol-2-yl)-p-cresol, about 225 g/mol) is the small workhorse of the class. Its low molecular weight keeps it compatible with coatings, adhesives, polyurethane and polycarbonate, and it is commonly dosed at 0.15–0.5 percent in plastics, rising toward 1–3 percent in clear industrial coatings where the film itself is the only shield.

UV-531: the benzophenone for polyolefins

UV-531 (2-hydroxy-4-octyloxybenzophenone, about 326 g/mol) carries an octyloxy tail that matches the low polarity of polyolefins. That makes it a standard pick for LDPE greenhouse film, PP woven tape and rotational moldings, typically at 0.25–1 percent. Its absorption also reaches somewhat deeper into the UV-B than most benzotriazoles.

What HALS do differently

HALS absorb almost no UV. The tetramethyl piperidine group instead runs a catalytic radical trap known as the Denisov cycle: the amine converts to a nitroxyl radical, captures an alkyl radical from the degrading polymer, then regenerates itself by reacting with a peroxy radical. One molecule cycles thousands of times, which is why effective loadings run low, commonly 0.05–0.5 percent. The two grades compared here sit at opposite ends of the molecular weight scale.

UV-770 (bis(2,2,6,6-tetramethyl-4-piperidyl) sebacate, about 481 g/mol) is the low-molecular-weight classic. High mobility lets it reach degradation sites quickly in PP and PE thick sections and in polyurethane. The same mobility works against it, since at high processing temperatures it can volatilize or bloom to the surface. UV-944, a polymeric HALS of roughly 2,600–3,400 g/mol, anchors into the compound instead. Low migration suits it to PP multifilament, HDPE tape and thin films, where loadings near 0.1 percent often carry the weathering warranty. One caution covers both grades: they are basic (N–H) HALS, and acidic species, from halogenated flame retardants to the HCl that PVC releases, can deactivate them, so halogen-rich systems deserve a screening trial first.

UV absorbers and HALS in one table

Grade Class MW, g/mol (typical) Mode of action Common uses Typical loading
UV-P Benzotriazole absorber ≈225 Absorbs UV, releases heat Coatings, PU, PC, PS 0.15–0.5%
UV-531 Benzophenone absorber ≈326 Absorbs UV, deeper UV-B reach PE, PP, EVA film; rotomolding 0.25–1%
UV-770 Low-MW HALS ≈481 Regenerative radical scavenging PP/PE thick sections, PU 0.05–0.5%
UV-944 Polymeric HALS ≈2,600–3,400 Radical scavenging, low migration PP fiber, tape, thin film 0.05–0.5%

The table explains the classic pairing. An absorber cuts the photon flux that reaches the bulk, and HALS mop up whatever radicals still form, so the combination routinely outperforms either family alone. Greenhouse film compounds commonly combine UV-531 with a HALS at a combined 0.3–0.8 percent. Below roughly 100 μm, recipes lean HALS-heavy, because the absorber’s optical path grows too short to matter. UV-622, a polymeric cousin of about 3,100 g/mol, appears in the same film and fiber duty.

Grade selection is also a shelf question. Our UV absorber and light stabilizer grades page lists ten of them, from UV-P, UV-9, UV-326, UV-327 and UV-360 through UV-531 and UV-571, plus the HALS UV-622, UV-770 and UV-944, all described for plastic, ink and coating systems. Outdoor compounds that also need whiteness pair these stabilizers with optical brighteners for plastics, since the brighteners themselves fade without stabilizer cover. The same selection logic runs across the plastic, ink and coating applications we supply.

Frequently asked questions

Can UV absorbers and HALS be used together?
Yes, and in weatherable compounds they usually should be. The absorber reduces incoming photons while the HALS quenches the radicals that still form, and many polyolefin recipes start near equal parts of each before outdoor exposure data settles the final ratio.

Which stabilizer works best in thin films?
A HALS, typically a polymeric grade such as UV-944. Below about 100 μm there is not enough path length for meaningful UV absorption, while radical scavenging does not depend on thickness at all.

Do HALS lose strength in PVC?
They can. UV-770 and UV-944 are basic N–H types, and acidic species such as the HCl that PVC releases tend to neutralize them. Halogenated or sulfur-containing systems warrant a screening trial before any long-term commitment.

From our catalog

Ningbo Ultra Color supplies UV absorbers and HALS within its additives range, with UV-P, UV-326, UV-531, UV-770 and UV-944 among the listed grades, alongside dyes, pigments and effect pigments. Every lot is checked against REACH SVHC and RoHS limits, and batch samples are kept for five years.

Scroll to Top