Polypropylene housewares, PVC trims and PET preforms all share one flaw: the resin carries a faint yellow cast that deepens after processing. Optical brighteners remove that cast with a trick no white pigment can copy. Dosed at a few hundred parts per million, they turn invisible ultraviolet light into a soft blue-violet glow, and the eye reads the result as clean, saturated white.

The Mechanism: UV In, Blue-Violet Out

Optical brighteners, which chemists call fluorescent whitening agents (FWAs), are fluorescent molecules rather than white pigments. While daylight or a UV lamp shines on the part, they absorb energy in the 340-380 nm band and re-emit it almost instantly as blue-violet fluorescence around 420-440 nm. OB-1, for instance, absorbs at roughly 374 nm and emits near 434 nm.

That blue-violet emission cancels the polymer’s yellow tone, so the surface measures whiter with no opaque coating at all. Two consequences follow. First, the effect only appears under light that contains UV, which is why a showroom LED lamp can hide what daylight reveals. Second, the dose is tiny. OB-1 datasheets typically recommend 200-500 g per tonne of polymer, which is 200-500 ppm.

OB-1, OB, KSN and KCB at a Glance

Four grades cover most whitening work in thermoplastics. The values below are typical for commercial datasheets; individual lots vary, so confirm against the supplier’s certificate of analysis.

Grade Chemistry class Melting point (typical) Best-fit resins and processes
OB-1 stilbene bis-benzoxazole (CAS 1533-45-5) 357-361°C PET, PA, PC, PS; extrusion above 280°C
OB oxadiazole (CAS 7128-64-5, C.I. FB 184) 196-203°C PVC, TPU, coatings, printing inks; below about 220°C
KSN benzoxazole, close structural cousin of OB-1 270-280°C PC, PA, synthetic fiber; high whiteness builds
KCB naphthalene bis-benzoxazole (CAS 5089-22-5, C.I. FB 367) 210-212°C EVA, PP, PE foam and shoe stock; cold blue-white cast

OB-1 versus OB: the temperature split

A melting-point gap of more than 150°C decides most jobs. OB-1 holds its performance through PET and PA extrusion at 280-300°C, with decomposition reported above 450°C, which is why masterbatch producers treat it as the high-temperature workhorse. It even ships in two shades, yellow and green, a difference commonly credited to crystal form, so the tint can be tuned to the resin. OB melts near 200°C. That confines it to processes staying below about 220°C, but in exchange it disperses readily in PVC, polyurethane, coatings and inks.

KSN versus KCB: intensity and hue

KSN sits chemically close to OB-1 yet melts roughly 80-90°C lower, and suppliers report that it builds more whiteness in polycarbonate at lower loading. That performance costs more per kilogram, so KSN tends to appear in premium engineering compounds rather than commodity packaging. KCB takes the opposite trade. Its naphthalene core pushes fluorescence toward a distinctly cold, blue white; it melts at 210-212°C, absorbs near 370 nm, and datasheets typically suggest 0.01-0.05%, which has made it a default in EVA foam, shoe stock and polyolefin housewares.

Match the Grade to the Resin

Choosing among optical brighteners in plastics comes down to two questions: how hot the process runs, and what shade of white the product needs. A barrel that runs above 250°C rules OB and KCB out immediately; a PVC calendar line at 180°C never needs the heat margin that OB-1 or KSN are paid for. Check the processing temperatures against typical resin and processing applications before committing a grade to a trial.

Masterbatch makers usually pre-disperse the powder in a resin-compatible carrier and let it down like any color concentrate. The selection discipline is the same as for masterbatch carriers for solvent dyes: match the carrier to the base polymer, hold the let-down ratio steady, and inspect dispersion of optical brighteners in plastics under a UV lamp rather than under office light.

Outdoor parts need a partner. The fluor itself fatigues under prolonged UV attack, so garden furniture and automotive trim pair the brightener with UV absorbers and HALS; benzotriazoles such as UV-326 and UV-327, or hindered amine grades like UV-770 and UV-944, are the common picks from the same additives shelf.

Ningbo Ultra Color treats optical brighteners as more than a side line. Its additives portfolio sits alongside the dye and pigment ranges and lists OB-1 in both shades, OB, KSN, KCB and FP127, plus UV absorbers. Raw materials are tested every batch, REACH SVHC and RoHS limits are checked, and retained samples are kept for five years.

FAQ

How much optical brightener does plastic need?

Far less than most formulators guess. Datasheets converge on 100-500 ppm: OB-1 at 200-500 g per tonne, KCB at 0.01-0.05%. Push past that range and whiteness stops improving or reverses, because concentrated fluor molecules re-absorb their own emission and the part takes on a greenish-yellow cast.

Why does my part look white outdoors but dull under LED light?

Fluorescence needs UV. Daylight carries plenty of it; many warm-white LEDs carry almost none, so the blue-violet contribution switches off and only the resin’s base color remains. Judge samples under D65 daylight or a UV inspection lamp, never under ceiling fixtures alone.

Which grade survives PET or PC processing?

OB-1 first, KSN as the upgrade. PET extrusion runs 270-300°C and PC molding sits near 280-320°C. OB-1 melts at 357-361°C and decomposes far higher, while KSN is reported to build stronger whiteness in PC. OB and KCB melt about 150°C lower and lose brightness long before the barrel reaches those temperatures.

Scroll to Top