Few colorants earn their keep at a fraction of one percent. Pigment Violet 23 is one of them. This carbazole dioxazine, known across the trade as dioxazine violet, delivers a bluish violet of unusual depth, and its tinting strength lets ink formulators dose it like a spice rather than a base ingredient. Measured product data for the grade lists 250°C heat stability, light fastness 7–8, and migration fastness 4 at 0.1% loading. On paper that sits a tier under the quinacridones. In an ink kitchen, the dioxazine usually wins on color per gram.

Tinting Strength Sets the Dose

The commercial case for PV23 rests on one property: tinting strength commonly rated around twice that of quinacridone violet. Deep masstone violets in flexographic and rotogravure packaging inks typically run at loadings around 1% or below, where classical organic violets need several times that figure for the same depth. The same strength makes PV23 a shading workhorse. A few tenths of a percent swings a phthalocyanine blue toward reddish blue, pulls a dull black toward a deeper blue-black, and builds the violet end of process color sets.

The dose is also the trap. Dioxazine crystals carry a high surface area, and dispersions pushed past typical letdown levels turn thick and stringy, a rheology ceiling that ink and coating formulators know well. Where high loading is unavoidable, the bluer variant PV37 is commonly positioned as the lower-strength, better-flowing alternative within the same chemistry.

The Measured Numbers for PV23

The values below come from the measured organic pigment data table: heat stability in °C, light fastness on the 1–8 scale, migration fastness at 0.1% loading, and suitability marks across twelve resin and application columns (● suitable, ○ limited, × unsuitable).

Grade Heat stability (°C) Light fastness (1–8) Migration FS 0.1% Resin suitability, 12 columns
Pigment Violet 23 Dioxazine 250 7–8 4 ● PVC, PE/PP, rubber, PUR; ○ PS, PA6, PET, PP fibers, PA fibers; × ABS, PC, PET fibers
Pigment Violet 19 Quinacridone 300 8 5 ● PVC, PE/PP, PS, rubber, PUR; ○ ABS, PET, PP fibers, PET fibers; × PA6, PC, PA fibers
Pigment Red 122 Quinacridone 300 8 5 ● PVC, PE/PP, PS, ABS, rubber, PUR; ○ PP fibers; × PA6, PET, PC, PET fibers, PA fibers

Read the matrix before the fastness row. PV23 carries full marks in PVC, polyolefins, rubber and polyurethane, limited marks in polystyrene, PA6 and PET, and crosses in ABS, polycarbonate and PET fiber. The quinacridone rows lean toward heat, holding full marks in polystyrene at 300°C-class stability. For ink work the distinction rarely bites, since liquid and paste systems process far below 250°C. In engineering polymers it decides the purchase.

Where the Doses Land: Inks and Industrial Coatings

Gravure and flexo are home ground. Solvent-borne and waterborne packaging inks use PV23 as the standard violet for flexible films, labels and folding cartons, where its strength holds formula cost down and its light fastness holds shade on the retail shelf. Offset inks call it up in smaller doses, for violet solids and for tone correction of blues. Over in industrial coatings applications, the pigment serves coil coatings, general industrial finishes and decorative paints that need a clean violet without automotive-grade weathering claims, and 250°C heat stability clears most bake schedules. What it does not forgive is abuse of the loading: above the typical dose, viscosity climbs and gloss drops.

Dioxazine or Quinacridone: Splitting the Violet Work

The two violet chemistries rarely compete for the same specification. PV23 takes the depth-per-gram work: inks, shading, masstone violets in vinyl and polyolefin systems. Quinacridones take the endurance work: PV19 and PR122 measure 300°C and light fastness 8, hold full suitability in polystyrene, and anchor exterior and automotive finishes. Polycarbonate rejects both families in the measured matrix. A fuller comparison of the quinacridone side, including the fiber-spinning grades, is in the quinacridone pigments guide.

FAQ

What dosage of Pigment Violet 23 gives a deep violet?

It depends on the system, but packaging inks typically reach full masstone depth at around 1% or below, and shading corrections run at a few tenths of a percent. The high tinting strength, commonly rated near twice that of quinacridone violet, is the reason for the small dose.

Is PV23 lightfast enough for exterior use?

The measured grade posts light fastness 7–8, high enough for many industrial and decorative exterior applications in masstone. For long-life exterior tints and automotive specifications, the 8-rated quinacridones PV19 and PR122 are the usual choice.

Can Pigment Violet 23 color engineering plastics?

Partly. The measured matrix gives limited marks in PA6 and PET and unsuitable marks in ABS and polycarbonate, with 250°C heat stability below the quinacridone line at 300°C. PV23 belongs in PVC, polyolefins, rubber and PUR; engineering polymers call for other chemistries.

Two Violet Chemistries, One Catalog

Ningbo Ultra Color supplies dioxazine PV23 alongside the quinacridone violets in its organic pigment range, with REACH and RoHS compliance checks on every lot and batch samples retained for five years. Buyers can match the pigment to the specification rather than bend the specification to one pigment.

Scroll to Top